Pinning and flush banding are the most common. There is some movement for fillers such as cyanoacrylate products. Most of these fillers become brittle over time and begin to leak again. Bell cracks are usually repaired with cyanoacrylate. Back in the old days musicians would fill cracks with hot wax. It worked.